1. Plastic treatment
PET, as a macromolecule, contains ester groups and is somewhat hydrophilic. The granular PET is relatively sensitive at high temperature. When moisture content goes beyond the limit, the molecular mass of PET will decline during processing. The products thereby manufactured will be colored and fragile. Therefore, prior to processing, the materials shall be dried for more than 4 hours at 150℃. Generally, they shall be dried for 3 to 4 hours at 170℃. Whether the materials are completely dry can be tested by air shot. In general, no more than 25% materials shall be recycled, and the recycled materials shall be thoroughly dried up.
2. Selection of injection molding machines
PET keeps stable for a shorter time after reaching the melting point, which is relatively high, so it is necessary to select injection systems with multiple temperature ranges which produce little heat for friction during plasticization. Besides, the actual weight of products (including drainage opening materials) shall not be lower than 2/3 of the injection quantity. In consideration of these requirements, Hwamda has developed small and medium-sized special plasticization systems for PET over the past years. The plasticization systems with a clamping force above 6300t/m2 can be used.
3. Mold and gate design
PET preforms are generally molded with hot runner molds. It is better the put a heat insulation plate between a mold and the formwork of an injection molding machine. The heat insulation plate shall be approximately 12mm thick and must withstand high pressure. The exhaust must be adequate to avoid local overheating or crack, whereas the vent depth generally shall not exceed 0.03mm, or else burr will easily form.
4. Hot melt glue temperature
Measure the temperature with air shot. The temperature ranges between 270℃ and 295℃. For enhanced GF-PET, the temperature can be set between 290℃ and 315℃.
5. Injection speed
Generally, the injection shall be fast to prevent too early solidification during injection. However, over speedy injection and high shear rate easily make materials fragile. The injection shall be generally completed within 4s.
6. Back pressure
The back pressure shall be as low as possible to avoid wear. Generally, it shall not exceed 100bar. In general, back pressure needn’t be used.
7. Residence time
The residence time must not be too long, to prevent molecular mass from declining. The temperature shall not exceed 300℃ if possible. If the device is shut down for fewer than 15min, only air shot will be needed. If the shutdown lasts more than 15min, clean the device with viscous PE, and decrease the barrel temperature to the PE temperature until the device is powered on again.
8. Notes
1) The recycled materials must not be too bulky, or else they will be easily piled up like “a bridge” in the feeding zone, thereby impacting plasticization. 2) If mold or material temperature is improperly controlled, “white fog” will be produced, thus making the products opaque. Low and uniform mold temperature, fast cooling and little crystallization make the products transparent.